Skip to content

PRECIMORA / Resource

Surface Finishes for Brass Turned Parts: As-Machined, Polished, Plated, or Lacquered?

The finish on a brass turned part is the first thing a buyer sees — and the last thing most drawings specify properly. A […]

The finish on a brass turned part is the first thing a buyer sees — and the last thing most drawings specify properly. A part can measure perfectly and still fail: its surface tarnishes in storage, a sealing face is too rough to seal, a plated layer peels, or a finish that looked right in the sample looks wrong after six months in service. Choosing a finish is not a cosmetic decision. This post shows you how to choose it by function: name what each surface has to do, and specify the finish — as-machined, polished, plated, passivated or lacquered — surface by surface.

A brass cylinder being turned to a mirror-smooth finish on a CNC lathe.

What the finish has to do

Every surface on a turned part has a job, and different jobs need different finishes. A bearing surface needs to be smooth enough for the mating part to slide without grabbing or wearing. A sealing face needs to be smooth enough for a seal to sit flat and hold pressure. An electrical contact needs a surface that conducts and does not oxidise into an insulator. A visible face needs to look right and stay looking right. A thread needs a surface that does not gall when the mating part is screwed in.

The mistake is to call out one finish for the whole part. A bushing whose bore is a bearing surface and whose outside is hidden inside a housing does not need the same finish on both. The bore may need Ra 0.4–0.8 µm, which Precimora lists as achievable on bearing surfaces on request, while the outside can stay as-machined at Ra 0.8–1.6 µm. Specifying the fine finish only where it works keeps the quote down and the part right. The discipline is the same as with tolerances: mark the finish where the function demands it, and leave the rest alone.

As-machined: the honest default

As-machined brass, at Ra 0.8–1.6 µm, is the standard finish for Precimora’s turned parts, and for most functional surfaces it is enough. A turned brass surface at this roughness is smooth to the touch, measures cleanly, and takes a thread well. It is also the cheapest finish, because it is what the turning operation produces without extra work.

The limitation is appearance and tarnish. Bare brass oxidises in air, and the bright gold surface dulls over weeks and months, faster in humid or polluted air. For a part hidden inside an assembly, that does not matter. For a visible part, or a part stored for months before assembly, it does — and that is when a protective finish earns its place. If the part will be assembled soon after delivery and is not visible in service, as-machined is usually the right call, and the money saved is real.

Polished: smooth, bright, and honest about its limits

Polishing takes a machined surface to Ra 0.4 µm or better, and it does two things: it makes the surface smoother, which helps sealing and sliding, and it makes it brighter, which helps appearance. For a sealing face or a visible face, polishing is often the simplest upgrade.

But polishing is not a coating. It does not stop tarnish — a polished brass surface will still oxidise, and because it starts brighter, the dulling is more visible. Polishing also removes material, so it must be done before the final dimensional check, and it cannot be applied selectively to a bore that is hard to reach. If the reason for polishing is appearance, ask whether a clear lacquer over the polished surface is also needed. If the reason is function — a seal or a bearing — polishing is the right tool, and the Ra value should be stated on the drawing for that surface only.

A pile of machined brass threaded inserts and bushings with a golden finish.

Plating: nickel, tin, and zinc

Plating adds a thin metal layer over the brass, and Precimora lists nickel, tin, or zinc as options, with nickel typically 5–25 µm. Each plating serves a different purpose, and choosing the wrong one is worse than choosing none.

Nickel is the hard, wear-resistant, corrosion-resistant option. It protects the brass underneath, gives a bright or satin silver appearance, and is a good base for further finishing. It is also the plating most often specified where the part must survive handling, wear, or a corrosive environment. The thickness matters: a nickel layer of 5 µm protects against tarnish, while a thicker layer is needed where wear is expected. State the thickness on the drawing, or at least the minimum, and confirm it during the review.

Tin is the electrical option. It solders easily, conducts well, and does not oxidise into an insulator the way bare copper does. For terminals, connectors, and electrical hardware, tin plating is often the right choice. It is softer than nickel and less wear-resistant, so it is not the choice for a surface that will be handled roughly or assembled repeatedly.

Zinc is the economical corrosion barrier, familiar from fasteners and fittings. It protects the brass and is cheap to apply, but it is not as hard as nickel and not as solderable as tin. It suits parts where corrosion protection matters and appearance and wear do not.

For any plating, two questions belong in the RFQ. First, what is the minimum thickness, and on which surfaces? Second, how is adhesion verified? A plating that peels is worse than no plating, and the supplier should be able to say how adhesion is checked. If the drawing does not state a thickness, the supplier will confirm a typical value during review — but a buyer who states the requirement gets a quote for the right plating, not a guess.

Passivation and lacquer: the quiet protectors

Chromate passivation and clear lacquer are the finishes buyers most often overlook, and they are often the cheapest way to solve a tarnish problem. Passivation forms a thin protective layer on the brass surface that slows oxidation without changing the dimensions or the appearance much. Clear lacquer coats the surface with a transparent film that keeps the bright brass look through storage and handling.

Lacquer is particularly useful for visible brass parts that will sit in stock before assembly. It preserves the appearance, but it is a coating that can scratch, and it must be compatible with any later soldering or assembly step — lacquer on a surface that will be soldered is a problem, not a protection. Say in the RFQ whether the part will be soldered, and on which surfaces, so the finish choice does not fight the assembly process.

How to state the finish in your RFQ

A good finish specification has three parts: which surface, what finish, and what value. “Polished, Ra 0.4 µm or better, bore only” is a specification. “Nice finish” is not. For plating, add the minimum thickness and the surfaces it applies to. For lacquer or passivation, state whether the part will be soldered or assembled in a way the coating could interfere with.

Also state the environment. A part that will live indoors in a dry cabinet needs a different finish from one that will sit in a humid warehouse for a year, or work outdoors, or handle water. The supplier cannot choose the right protection without knowing what the part will face, and the finish that is right for one environment is wrong for another.

Polished brass threaded cylindrical components with smooth turned contours, disassembled on a white background.

Buyer questions, answered

Is as-machined brass good enough, or do I need a finish? — As-machined brass, at Ra 0.8–1.6 µm, is the standard finish for Precimora’s turned parts and is enough for most functional surfaces. Its limitation is appearance and tarnish: bare brass oxidises in air and the bright gold surface dulls over weeks and months, faster in humid or polluted air. For a part hidden inside an assembly and assembled soon after delivery, as-machined is usually the right call.

When should I choose polishing? — When the reason is function — a sealing face or a bearing surface that needs Ra 0.4 µm or better — or appearance on a visible face. Polishing is not a coating: it does not stop tarnish, and because a polished surface starts brighter, the dulling is more visible. If the reason is appearance, ask whether a clear lacquer over the polished surface is also needed.

Nickel, tin or zinc plating — which one? — Nickel is the hard, wear-resistant, corrosion-resistant option, typically 5–25 µm, for parts that must survive handling, wear or a corrosive environment. Tin is the electrical option — it solders easily and conducts well — for terminals, connectors and electrical hardware. Zinc is the economical corrosion barrier where appearance and wear do not matter. For any plating, state the minimum thickness and the surfaces it applies to, and ask how adhesion is verified.

My parts will sit in stock for months before assembly — what protects them? — Say so in the RFQ and ask about chromate passivation or clear lacquer. Passivation forms a thin protective layer that slows oxidation without changing the dimensions or the appearance much. Lacquer keeps the bright brass look through storage and handling — but it is a coating that can scratch, and it must be compatible with any later soldering or assembly step, because lacquer on a surface that will be soldered is a problem, not a protection.

Common pitfalls and how to avoid them

The most common pitfall is specifying one finish for the whole part, which pays for a fine finish on surfaces that do not need it. Mark the finish per surface.

The second is choosing a finish for appearance and forgetting tarnish. Bare and polished brass dull in storage; if the part will sit before assembly, say so and ask about lacquer or passivation.

The third is plating without a thickness. A plating callout with no thickness is a guess — state the minimum, at least for nickel, and confirm it in the review.

The fourth is lacquer on a surface that will be soldered. Lacquer and solder do not mix; state the assembly process in the RFQ.

The fifth is assuming the finish is included in the base price. Polishing, plating, and lacquer are operations with their own cost, and they should be visible in the quote. If the quote does not mention the finish, ask — a missing finish in the quote usually means it was not included.

Finish selector: match the surface job to the finish

A quick-reference table built from this post. Find the surface’s job, then the finish:

Surface jobFinish to specify
Bearing or sliding surfacePolished, Ra 0.4 µm or better — or as-machined Ra 0.8–1.6 µm if the function allows
Sealing facePolished, with the Ra value stated for that surface only
Electrical contact, terminal, connectorTin plating — solders easily, conducts well, does not oxidise into an insulator
Handling, wear, or corrosive environmentNickel plating, minimum thickness stated (typically 5–25 µm)
Economical corrosion barrierZinc plating
Visible part stored before assemblyPolished plus clear lacquer, or chromate passivation
Hidden part assembled soon after deliveryAs-machined

Two rules govern the table. First, one finish per surface, never one finish for the whole part — a bushing whose bore is a bearing surface and whose outside is hidden inside a housing does not need the same finish on both. Second, the finish appears as its own line in the quote, so its cost is visible: polishing, plating and lacquer are operations with their own cost, and a quote that does not mention the finish usually means it was not included.

Buyer checklist

  1. Each functional surface is named: bearing, sealing, electrical contact, visible, or hidden.
  2. The finish is called out per surface, not as one finish for the whole part.
  3. Roughness values are stated where they matter (for example Ra 0.4–0.8 µm on bearing surfaces, Ra 0.8–1.6 µm as-machined elsewhere).
  4. Plating is specified by type and minimum thickness, and on which surfaces.
  5. Tarnish and storage time are stated, so lacquer or passivation can be considered.
  6. Any soldering or assembly step that a coating could interfere with is stated.
  7. The environment in service is described: indoor, humid, outdoor, or water contact.
  8. The finish appears as its own line in the quote, so its cost is visible.

Send the drawing and state the finish per surface — which faces seal, slide, conduct, or show — in the RFQ at https://precimora.com/request-a-quote/ — the quote is promised in 24–48h.

Drawing-led production

Have a part ready for production?

Send your drawing and requirements for engineering review.

Upload DrawingTalk to an Engineer
WhatsApp